Reductive ammonia leaching method was used to recover Cu and Co from heterogenite. The influences of the reductant quantity, leaching temperature, the concentration ratio of NH_3 to (NH_4)_2SO_4, leaching time and liquid-solid (L/S) ratio on leaching rate of cobalt and copper were investigated. The optimal conditions at which the leaching rate of copper and cobalt were 96.07%, 98.24% respectively and that of Fe, Mg and Al were almost 0 were as follows: time = 5 h, T = 50°C, the amount of ammonia is 1.2 times of theorrtical, C(NH_3):C [(NH_4)_2SO_4] =1:3, L/S ratio = 3:1, and the dosage of Na_2SO_3 is 0.5 times of the heterogenite's mass.
机译:还原氨浸出方法用于回收Cu和Co的异化物。研究了还原剂量,浸出温度,NH_3至(NH_4)_2SO_4,浸出时间和液体 - 固体(L / S)比的影响,对钴和铜的浸出速率的浸出速率。铜和钴的浸出速率分别为96.07%,98.24%,Fe,mg和Al的最佳条件差别如下:时间= 5 h,t = 50℃,氨的量1.2次ortratical,C(NH_3):C [(NH_4)_2SO_4] = 1:3,L / S比率= 3:1,Na_2SO_3的剂量为超源性物质的0.5倍。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号