The thermal simulation experiments of X80 pipeline steel were performed using Gleeble 1500 thermomechanical simulator. The controlled rolling and controlled cooling experiments were used to investigate the effect of cooling rate on the microstructures and mechanical properties of X80 pipeline steel. The results show that the cooling rate plays an important role in the ferrite grain size and the volume fraction of granular bainite. In order to obtain good comprehensive mechanical properties, it is necessary that the cooling rate should be 12~20°C/s.
机译:使用GLEEBLE 1500热机械模拟器进行X80管线钢的热仿真实验。控制轧制和受控冷却实验用于研究冷却速率对X80管道钢的微观结构和机械性能的影响。结果表明,冷却速率在铁氧体晶粒尺寸和粒状贝氏体的体积分数中起重要作用。为了获得良好的综合机械性能,冷却速度应为12〜20°C / s。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号