The Changes of Thickness and Tearing Behavior of Tencel Fabrics Treated With Different Time by Plasma

机译:等离子体不同时间处理Tencel织物的厚度和撕裂行为的变化

获取原文

摘要

Tencel fabrics were treated with low pressure plasma with air for different treatment time. The samples were tested their thickness and calculated each mean value of fabrics treated with different time. The result indicated that samples became thicker with the prolonged plasma treatment time. The samples were also divided into two groups and tore along warp and weft direction, respectively, to measure the influence of plasma treatment time on the tearing strength. The result of the measurement implied that the tearing strength of samples treated 1 minute by plasma decreased dramatically, when they were compared with the untreated ones. However, the decrease of the tearing strength became slight when the plasma treatment increased to 5, 10 and 20 minutes.
机译:用空气用低压等离子体处理Tencel织物,用于不同的处理时间。测试样品厚度并计算出不同时间处理的织物的每个平均值。结果表明,样品与延长的血浆治疗时间变厚。分别将样品分为两组和沿经纱和纬向方向分为两组,以测量等离子体处理时间对撕裂强度的影响。测量结果暗示,当与未处理的那些相比,通过等离子体处理1分钟的样品的撕裂强度急剧下降。然而,当血浆处理增加至5,10和20分钟时,撕裂强度的降低变得轻微。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号