The preparation of ultrafine-grained alumina ceramics by the fast sintering technique Self-propagating High-temperature Synthesis plus Quick Pressing (SHS-QP) method was reported.The reaction heat generated by combustion reaction was applied to act as a high temperature source.An alumina compact was loaded inside the combustion reactants,which form a “SHS-furnace”,and great mechanical pressure was applied when the temperature reached the maximum.Dense ultrafine-grained alumina ceramic was prepared using a lower heating rate (900 °C/min),and the effects of sintering time,and pressure on the densification and grain size were discussed.Within a short sintering time of 3 min,full-density alumina ceramics with ultrafine-grained structure are obtained under a pressure of 120 MPa.
机译:报道了通过快速烧结技术制备超细粒化氧化铝陶瓷,自展开高温合成加快压制(SHS-QP)方法。施加燃烧反应产生的反应热量作为高温源。在燃烧反应物内装载氧化铝结构,该燃烧反应物形成“SHS-炉”,当温度达到最大的加热速率时,当温度达到最大的超细颗粒氧化铝陶瓷时施加了很大的机械压力(900℃/ min )讨论了烧结时间和压力对致密化和晶粒尺寸的影响。在短的烧结时间为3分钟,在120MPa的压力下获得具有超细凝聚结构的全密度氧化铝陶瓷。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号