Electrolyte Effect to Copolymer Grafting of Starch onto Natural Rubber Using Glow Discharge Electrolysis Plasma (GDEP) Method

机译:使用辉光放电电解等离子体(GDEP)法将淀粉与天然橡胶共聚到天然橡胶的电解质效应

获取原文

摘要

Natural rubber has an important role in many applications such as tyre products due to excellent elasticity and high friction causing wear on the tire and leading to energy dissipation in the form of heat and noise. Although reinforcing both inorganic and organic fillers can be a solution, it generally needs expensive coupling agent. Finding an excellent coupling agent by considering to environmentally friendly materials and economic aspect, is an interesting study. This study reported modification of natural rubber through copolymer grafting of starch onto natural rubber latex using Glow Discharge Electrolysis Plasma (GDEP) with varying of electrolyte. The experimental indicated that the electrolytes generally give significant effect to percent yield of the hybrid natural rubber-starch product. The highest percent yield is obtained from adding KCl. Addition of the divalent salts such as MgCl_2 and CaCl_2 disturbs the process due to reaction the salts with stabilizing system in natural rubber latex. Addition of NaOH is able to enhance the reaction performance with considering the radical elements recombination. The starch part as polar part and the natural rubber as non polar part building up the hybrid natural rubber-starch products, correlate with hydrophilicity and degradation of the both parts. This study results in the lowest contact angle of 54.8°, the highest percent yield of 8.6 %,, and the highest starch content in the product of 1.6%.
机译:天然橡胶在许多应用中具有重要作用,如轮胎产品,因为造成了良好的弹性和高摩擦,导致轮胎磨损,导致热量和噪音的形式耗散。虽然增强无机和有机填料可以是溶液,但它通常需要昂贵的偶联剂。通过考虑环保材料和经济方面,寻找优秀的偶联剂是一个有趣的研究。本研究报告了通过具有不同电解质的辉光放电电解等离子体(GDEP)来改变天然橡胶通过淀粉的共聚物嫁接到天然橡胶胶乳上。实验表明,电解质通常对杂化天然橡胶 - 淀粉产品的百分比产生显着影响。从加入KCl获得最高产率。添加二价盐,例如MgCl_2和CaCl_2,由于在天然橡胶胶乳中与稳定系统反应盐的反应,使得该方法进行扰乱。添加NaOH的添加能够考虑自由基元素重组来增强反应性能。淀粉部分作为极地部分和天然橡胶作为非极性部分构建杂交天然橡胶淀粉产品,与双方的亲水性和降解相关。该研究导致最低的接触角为54.8°,产率最高为8.6%,最高淀粉含量为1.6%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号