粒度差异对氧压酸浸闪锌矿浸出效率的影响

         

摘要

The test is on the basis of the on-site process in the Oxygen pressure acid leaching workshop of Danxia smelter .After technical improvement ,the content of -40μm can be increased from 65% to 83%through the secondary vertical agitating mill .The pulp before and after grinding was taken respectively as raw materials of leaching ,and then small oxygen pressure acid leaching sphalerite experiment was carried out in the laboratory .The experimental results show that ,as the size of leaching material become smaller ,the leaching efficiency become higher .Along with the diminution of the size of leaching material ,the residue rate of leaching residue reduce ,the grade of Zn in leaching residue also reduce ,that brings recovery ratio’ s increase of Zn resources ,reduces the waste of resources .100000 tons of zinc ingots can be produced per annum in Danxia smelter former ,and the prices of Zn ingot about 14500 yuan per ton ,if the leaching efficiency increased by 2% ,earnings of Danxia smelter will increase around 29 million each year .%本试验以丹霞冶炼厂氧压浸出车间现场流程为基础。经过技术改进后的二段砂磨机将矿浆中-40μm含量由65%提高到83%,取磨矿前后矿浆为浸出物料,在实验室进行小型氧压酸浸闪锌矿试验。结果证实了浸出物料变细,浸出效率会提高。浸出物料变细后,浸出渣的渣率降低,浸出渣中Zn品位下降,锌资源回收率提高,减少了资源浪费。以试验结果提高2%的浸出效率来算,冶炼厂原年生产10万t锌锭,每吨1.45万元来计,每年将提高厂收益2900万元左右。

著录项

  • 来源
    《中国矿业》 |2014年第10期|118-120|共3页
  • 作者单位

    武汉科技大学冶金矿产资源高效利用与造块湖北省重点实验室;

    湖北武汉430081;

    武汉科技大学冶金矿产资源高效利用与造块湖北省重点实验室;

    湖北武汉430081;

    长沙矿冶研究院有限责任公司;

    湖南长沙410012;

    武汉科技大学冶金矿产资源高效利用与造块湖北省重点实验室;

    湖北武汉430081;

    武汉科技大学冶金矿产资源高效利用与造块湖北省重点实验室;

    湖北武汉430081;

    武汉科技大学冶金矿产资源高效利用与造块湖北省重点实验室;

    湖北武汉430081;

  • 原文格式 PDF
  • 正文语种 chi
  • 中图分类 有色金属矿选矿;
  • 关键词

    砂磨机; 磨矿; 氧压酸浸; 浸出效率;

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号