Bending fatigue characteristics of nanohoneycomb structures

机译:纳米蜂窝结构的弯曲疲劳特性

获取原文
获取原文并翻译 | 示例
           

摘要

Nanohoneycomb beam structures of Anodic Aluminum Oxide (AAO) were fabricated by a two-step anodization process. The bending fatigue properties of nanohoneycomb structures were measured using a Nano-Universal Testing Machine (UTM) under cyclic three-point bending. The mean values of the experimental results were compared with several single load level fatigue life prediction equations with good agreement, although there were large deviations of experimental fatigue life data among samples with the same load level. There were small increments of resultant displacements during cyclic loading. The present results can be used as a design guideline in applications of nanohoneycomb structures.
机译:通过两步阳极氧化工艺制备了阳极氧化铝纳米蜂窝结构。使用纳米通用试验机(UTM)在循环三点弯曲下测量纳米蜂窝结构的弯曲疲劳特性。将实验结果的平均值与几个单载荷水平疲劳寿命预测方程进行了比较,尽管它们在相同载荷水平下的实验疲劳寿命数据之间存在较大偏差,但这些方程具有良好的一致性。在循环荷载作用下,位移的增量很小。本研究结果可作为纳米蜂窝结构应用中的设计指南。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号