This study introduces the preparation of sub-micron composite particles of phloroglucinol-Fe and Cl-20 (Fe-Ph/Cl-20) with a spherical shape using spray drying technology. The influences of solution concentration and temperature on the morphology and particle size of the Fe-Ph/Cl-20 particles were studied using a scanning electron microscope (SEM) and a laser particle analyzer. The results show that when the concentration (ethyl acetate as solvent) of Fe-Ph/Cl-20 (0.3 g?:?10 g) is 10.30 g/100 g and the temperature is 80 °C, the Fe-Ph/Cl-20 particles are well-defined spherical particles ( D _(50) 958.96 nm and D _(90) 1647.63 nm). Thermal decomposition of Fe-Ph/Cl-20 is studied using a differential scanning calorimeter (DSC). The DSC illustrates that the apparent activation energy of Fe-Ph/Cl-20 is reduced by 41.9 kJ mol ~(?1) . The spray drying technology provides theoretical support and introduces a new direction for preparing the sub-micron composite particles of high explosives and combustion catalysts.
机译:本研究介绍了使用喷雾干燥技术的球形形状制备甘黄油-FE和Cl-20(Fe-pH / Cl-20)的亚微米复合颗粒。使用扫描电子显微镜(SEM)和激光粒子分析仪研究了溶液浓度和温度对Fe-pH / Cl-20颗粒的形态和粒度的影响。结果表明,当Fe-pH / Cl-20的浓度(乙酸乙酯作为溶剂)(0.3g≤10g)为10.30g / 100g时,温度为80℃,Fe-pH / Cl -20颗粒是明确定义的球形颗粒(D _(50)958.96nm和D _(90)1647.63nm)。使用差示扫描量热计(DSC)研究Fe-pH / Cl-20的热分解。 DSC说明Fe-pH / Cl-20的表观活化能量减少41.9kJ摩尔〜(α1)。喷雾干燥技术提供理论支持,并引入制备高爆炸物和燃烧催化剂的亚微米复合颗粒的新方向。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号