Fatigue Resistance of HPS-485W (70 W) Continuous Plate with Punched Holes

机译:带穿孔的HPS-485W(70 W)连续板的抗疲劳性

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Twenty-nine specimens were tested to investigate the fatigue resistance of high-performance steel (HPS-485W) (70 W) continuous plate with punched holes. Specimen thickness, hole diameter, and method used for creating the holes were varied to examine their effect upon fatigue resistance of punched connections utilizing high performance steel. Eight of the 29 specimens were drilled or subpunched and reamed specimens, all of which rated as Category B details. The remaining 21 specimens had punched holes and rated considerably below a Category B. Results from this investigation suggest that current restrictions mandated by some state DOTs concerning punching holes are not overly restrictive when HPS-485W (70 W) is utilized. Performance of drilled and subpunched and reamed specimens met (or exceeded) 2004 AASHTO requirements for Category B details.
机译:测试了29个样品,以研究具有穿孔的高性能钢(HPS-485W)(70 W)连续板的耐疲劳性。改变试样的厚度,孔的直径和用于制造孔的方法,以检查它们对使用高性能钢的冲压连接的疲劳强度的影响。在29个样品中,有8个是经过钻孔或再打孔和扩孔的样品,所有这些都被定为B类细节。其余的21个样品带有打孔,并且其额定值大大低于B类。这项调查的结果表明,当使用HPS-485W(70 W)时,某些州DOT对打孔的限制并不过于严格。钻孔,再穿孔和扩孔试样的性能达到(或超过)2004 AASHTO B类标准的要求。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号