A series of highly Er~(3+) /Yb~(3+) co-doped fluoroaluminate glasses were investigated in order to develop a microchip laser at 1.54 mu m under 980 nm excitation. Measurements of absorption, emission and up-conversion spectra were performed to examine the effect of concentration quenching on spectroscopic properties. In the glasses with Er3 + concentrations below 10 percent (mol fraction), concentration quenching is low and the Er~(3+) /Yb~(3+) co-doped fluoroaluminate glasses gave stronger fluorescence of 1.54 mu m from the ~4I_(13/2) - > ~4I_(15/2) transition than those of Er~(3+) singly-doped glasses. In the glass with Er~(3+) concentrations above 10 percent, concentration quenching of 1.54 mu m obviously occurs more than that of the Er~(3+) singly-doped samples because of the back energy-transfer from Er~(3+) to Yb~(3+). To obtain the highest emission efficiency at 1.54 mu m, the optimum doping-concentration ratio of Er~(3+)/Yb~(3+) is found to be approximately 1:1 in mol fraction when the Er~(3+) concentration is less than 10 percent.
机译:为了开发在980nm激发下1.54μm的微芯片激光器,研究了一系列高Er〜(3 +)/ Yb〜(3+)共掺杂氟铝酸盐玻璃。进行吸收,发射和上转换光谱的测量以检查浓度猝灭对光谱性质的影响。在Er3 +浓度低于10%(摩尔分数)的玻璃中,浓度猝灭很低,Er〜(3 +)/ Yb〜(3+)共掺杂氟铝酸盐玻璃从〜4I_发出的荧光更强,为1.54μm。 (13/2)->〜4I_(15/2)的跃变比Er〜(3+)单掺杂玻璃的跃迁。在Er〜(3+)浓度高于10%的玻璃中,由于Er〜(3 +)到Yb〜(3+)。为了在1.54μm处获得最高的发射效率,当Er〜(3+)时,Er〜(3 +)/ Yb〜(3+)的最佳掺杂浓度比约为1:1(摩尔比)。浓度小于10%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号