Evaluation of the fit of metal ceramic restorations fabricated with a pre-sintered soft alloy

机译:评估用预烧结软合金制造的金属陶瓷修复体的配合

获取原文
获取原文并翻译 | 示例
           

摘要

Statement of problem. Fit is an important factor influencing the success or failure of restorations. Recently, there has been increasing use of a newly developed pre-sintered soft alloy for use in computer-aided design and computer-aided manufacturing (CAD-CAM) of cobalt-chromium alloys for the fabrication of metal ceramic restorations. However, almost no studies are available on the fit of restorations fabricated in this way.
机译:问题陈述。合适度是影响修复成功与否的重要因素。最近,越来越多地使用新开发的预烧结软合金,用于钴铬合金的计算机辅助设计和计算机辅助制造(CAD-CAM),以制造金属陶瓷修复体。但是,几乎没有关于以这种方式制作的修复体适合性的研究。