Thermal condensation of glucose-diammonium phosphate in wood at 160 and 190pC will protect wood against fire and decay in one treatment using an aqueous system. For fire protection, treatments at 160 or 190pC led to low flammability as evidenced by fire-tube tests. For nonleached wood, weight losses were 1.9, 2.0, and 2.0% with chemical retentions of 56.7, 44.7, and 64.7%, respectively, for 2-, 4-, and 6-h heating; and for leached wood, weight losses of 5.1, 3.8, and 1.5% with chemical retentions of 24.5, 24.1, and 45.6%, respectively, for 2-, 4-, and 6-h heating compared with 18.8% weight loss for diammonium phosphate-treated wood with chemical retention of 19.4%. The control had 84.4% weight loss. For decay protection, heat treatment at 190pC for 30 min after 2-wk water leaching also prevents degradation by brown and white rot fungi. Weight loss by Gloeophyllum trabeum (Gt) was 0.4% with 19.5% chemical retention, and weight loss by Trametes versicolor (Tv) was 1.5% with 17.8% chemical retention. The control had 30.6 and 36.8% weight losses by Gt and Tv, respectively.
机译:在使用含水系统的一种处理中,葡萄糖和磷酸二铵在160和190pC时在木材中的热缩合可保护木材免于着火和腐烂。在防火方面,通过火管测试证明,在160或190pC的温度下进行处理会导致易燃性低。对于非沥滤木材,加热2小时,4小时和6小时时,重量损失分别为1.9%,2.0%和2.0%,化学保留率分别为56.7%,44.7%和64.7%;对于浸提的木材,加热2小时,4小时和6小时的重量分别减少了5.1%,3.8%和1.5%,化学保留率分别为24.5%,24.1和45.6%,而磷酸二铵的重量减少了18.8%。处理的木材,化学保留率为19.4%。对照具有84.4%的体重减轻。为了防止腐烂,在2周水浸出后在190pC热处理30分钟也可以防止棕色和白色腐烂真菌降解。球墨茶(Gt)的重量损失为0.4%,化学保留率为19.5%,而云芝(Tv)的重量损失为1.5%,化学保留率为17.8%。对照通过Gt和Tv分别具有30.6和36.8%的重量损失。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号