During production of primary and secondary aluminum, various amounts (in some cases up to 200 kg) of aluminum dross, a mixture consisting of molten aluminum metal and different oxide compounds (the nonmetallic phase), are skimmed per tonne of molten metal. To preserve the maximum aluminum content in hot dross for further extraction, it is necessary to cool the dross immediately after skimming. One way to do this is to press the skimmed hot dross in a press. In this process, the skimmed dross is transformed into so-called pressed skulls, with characteristic geometry convenient for storage, transport, or further in-house processing. Because of its high aluminum content-usually between 30% and 70%-pressed skulls represent a valuable source of aluminum and hence are in great demand in the aluminum recycling industry. Because pressed skulls are generally valued on a free-metal recovery basis, which is influenced by the yield of recovery, or in other words, by the quality of the recycling process, it was recognized as important and useful to develop a method of fast and cost-effective nondestructive measurement of the free aluminum content in pressed skulls, independent of the technology of pressed skulls recycling.
机译:在生产一次和二次铝的过程中,每吨熔融金属撇去各种量(在某些情况下可达200​​千克)的铝渣,铝渣是由熔融铝金属和不同氧化物化合物(非金属相)组成的混合物。为了保留热渣中的最大铝含量以便进一步提取,撇渣后必须立即冷却渣。一种方法是在压榨机中压榨脱脂渣。在此过程中,脱脂渣被转变为所谓的压制头骨,其特征几何形状便于存储,运输或进一步内部加工。由于铝含量很高(通常在30%至70%之间),受压头骨代表了铝的宝贵来源,因此在铝回收行业中需求量很大。由于压制的头骨通常是根据游离金属的回收率来评估的,这受回收率的影响,换句话说,受回收过程的质量的影响,因此,人们认为开发一种快速,高效的方法非常重要且有用。经济实用的压制颅骨中游离铝含量的无损测量,与压制颅骨回收技术无关。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号