The effects of chemical treatments and modifications on the tensile properties of ring- and rotor-spun cotton yarns is discussed. The rotor-spun yarns treated with zinc chloride show a higher tenacity at low stretch levels compared to sodium hydroxide, whereas with sodium hydroxide, the rotor-spun yarns show higher tenacity at higher stretch levels compared with zinc chloride. The aqueous-treated rotor-spun yarns show a higher change in tenacity compared to ring-spun yarns. Sodium hydroxide-treated yarns before resin treatment show a higher retained tenacity compared to zinc chloride-treated yarns. The substitution treatment after swelling and stretching to 100% shows a higher tenacity than that of the slack substituted yarns. (C) 1995 John Wiley and Sons, Inc. [References: 33]
机译:讨论了化学处理和改性对环锭纺和转杯纺棉纱拉伸性能的影响。与氯化钠相比,用氯化锌处理的转杯纺纱在低拉伸水平下显示出更高的强度,而在氢氧化钠条件下,与氯化锌相比,用氢氧化钠处理的转杯纺纱具有更高的强度。与环锭纺纱相比,经水处理的转杯纺纱表现出更高的强度变化。与氯化锌处理的纱线相比,树脂处理之前的氢氧化钠处理的纱线显示出更高的保留韧度。溶胀和拉伸至100%后的替代处理显示出比松弛的替代纱线更高的韧性。 (C)1995 John Wiley and Sons,Inc. [参考:33]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号