摘要

The aim of this report is to analyze the microstructures of glass-ceramics of the IPS Empress?2 and IPS Empress? systems by scanning electron microscopy. The main properties of the glass-ceramics were determined and compared to each other. The flexural strength of the pressed glass-ceramic (core material) was improved by a factor of more than three for IPS Empress? 2 (lithium disilicate glass-ceramic) in comparison with IPS Empress? (leucite glass-ceramic). For the fracture toughness, the K_(IC) value was measured as 3.3 +- 0.3 MPa centre dot m~(0.5)for IPS Empress?2 and 1.3 +- 0.1 MPa centre dot m~(0.5) for IPS Empress?. Abrasion behavior, chemical durability, and optical properties such as translucency of all glass-ceramics fulfill the dental standards. The authors concluded that IPS Empress?2 can be used to fabricate 3-unit bridges up to the second premolar.
机译:本报告的目的是分析IPS Empress?2和IPS Empress?的玻璃陶瓷的微观结构。系统通过扫描电子显微镜观察。确定了玻璃陶瓷的主要性能并进行了比较。对于IPS Empress ?,压制的玻璃陶瓷(芯材)的抗弯强度提高了三倍以上。 2(二硅酸锂玻璃陶瓷)与IPS Empress的比较? (白晶玻璃陶瓷)。对于断裂韧性,对于IPS Empress?2而言,K_(IC)值为3.3±0.3 MPa中心点m〜(0.5),对于IPS Empress?而言,为1.3±0.1 MPa中心点m〜(0.5)。所有玻璃陶瓷的耐磨性,化学耐久性和光学特性(如半透明性)均符合牙科标准。作者得出的结论是,IPS Empress?2可用于制造直至第二颗前磨牙的3单元桥。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号