A new macromolecular coupling agent, low-molecular-weight polybutadiene liquid rubber (LMPB)-glycidyl methacrylate (GMA), was synthesized using solution polymerization initiated by benzoyl peroxide (BPO). The molecular structure was confirmed by FTIR and NMR. This macromolecular LMPB-GMA was used for surface modification of silicon nitride (Si _3N _4) nanopowder in n-heptane, chloroform, ethyl acetate, and DMF, respectively. LMPB-GMA and modified nano-Si _3N _4 were systematically investigated by FTIR, NMR, TGA, and TEM. The results showed that LMPB-GMA bonded and formed an organic coating layer onto the surface of nanosized Si _3N _4 particles. The polarity of the solvents plays an important role in this process. Strong or weak polar both affect the results. The dosage loading of LMPB-GMA is 12 wt% of nanosized Si _3N _4. Nanosized Si _3N _4 modified in ethyl acetate has better dispersibility and stability than that modified in n-heptane or DMF. TEM pictures also reveal that modified nano-Si _3N _4 possesses good dispersibility.
机译:利用过氧化苯甲酰(BPO)引发的溶液聚合反应合成了一种新的大分子偶联剂,低分子量聚丁二烯液态橡胶(LMPB)-甲基丙烯酸缩水甘油酯(GMA)。分子结构通过FTIR和NMR确认。该大分子LMPB-GMA用于分别在正庚烷,氯仿,乙酸乙酯和DMF中对氮化硅(Si _3N _4)纳米粉进行表面改性。通过FTIR,NMR,TGA和TEM对LMPB-GMA和修饰的纳米Si _3N _4进行了系统研究。结果表明,LMPB-GMA在纳米Si _3N _4纳米粒子的表面上结合并形成有机涂层。溶剂的极性在此过程中起重要作用。强极性或弱极性都会影响结果。 LMPB-GMA的剂量负载为纳米Si _3N _4的12 wt%。乙酸乙酯中改性的纳米Si_3N_4比正庚烷或DMF改性的硅具有更好的分散性和稳定性。 TEM照片还表明,改性的纳米Si _3N _4具有良好的分散性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号