Fe100-xNix alloys were obtained by a mechanical alloying technique (MA) from elemental metals. The alloys consist of: single body-centered cubic phase (bcc) at nickel concentrations less than or equal to 22 at.%, single face-centered cubic phase (Fcc) - at x > 28 at.% and two of these phases - at 22 less than or equal to x less than or equal to 28 at.%. Annealing results in formation of single fcc phase structure in the samples with x greater than or equal to 22 at.%. According to the Mossbauer spectrometry data these annealed alloys with 22-28 at.% Ni were not ferromagnetic at room temperature. Cooling austenitic samples in liquid nitrogen as well as mechanical deformation stimulated austenite-marten site transformation accompanied by the appearance of ferromagnetism. (C) 2001 Elsevier Science B.V. All rights reserved. [References: 21]
机译:Fe100-xNix合金是通过机械合金化技术(MA)从元素金属中获得的。合金包括:镍浓度小于或等于22 at。%的单心立方立方相(bcc),x> 28 at。%的单面心立方立方相(Fcc)和其中两个相- 22小于或等于x小于或等于28 at。%。退火导致样品中x大于或等于22 at。%的单fcc相结构的形成。根据Mossbauer光谱数据,这些具有22-28 at。%Ni的退火合金在室温下不是铁磁性的。在液氮中冷却奥氏体样品以及机械变形会引起奥氏体-马氏点转变,并伴有铁磁性。 (C)2001 Elsevier Science B.V.保留所有权利。 [参考:21]

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号