This paper reports hardness and abrasive wear resistance test results from a wide range of WC-Co alloys, varying in cobalt content as well as WC grata size. The results show that the abrasive wear resistance increases with increasing hardness and that the rate of increase is higher for larger WC grain sizes. The increase in abrasive wear resistance was found to be parabolic up to a critical hardness value and exponential above that value. The transition from parabolic to exponential behaviour was found to occur at the same contiguity value for all grain sizes, which suggests that at that contiguity value the WC skeleton becomes continuous in all WC-Co alloys.