Bi2Sr2CaCu2O8+delta (Bi-2212) thin films were grown on MgO (1 0 0) using 1064 nm infrared pulsed laser deposition with post heat treatment. The material arrives at the substrate surface with characteristic spheroidal morphology. Smooth, homogeneous and highly c-axis oriented films were obtained after heat treatment. Using infrared laser as excitation, the stoichiometry of the target is preserved on the film. However, the films were apparently under-doped.
机译:使用1064 nm红外脉冲激光沉积和后热处理,在MgO(1 0 0)上生长Bi2Sr2CaCu2O8 +δ(Bi-2212)薄膜。材料以特征性的球状形态到达基板表面。热处理后可获得光滑,均匀且高度c轴取向的薄膜。使用红外激光作为激发,靶的化学计量被保留在膜上。但是,这些薄膜显然掺杂不足。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号