High-resolution pyrolysis gas chromatography-mass spectrometry (HRPyGC-MS) and Fourier transform infrared spectrometry (FTIR) were used to study the structures of the chlorinated natural rubbers (CNR) prepared by two different processes. The results indicate that the fine structures of CNR prepared from "latex" and "solution" processes are different, whereas their basic structures are similar. The molecule of CNR from the "latex" process contains a few carboxyl and carbonyl groups. The rings on CNR molecular chains should be hexatomic rings. The optimum pyrolytic temperature for CNR is 445degreesC, with an available range from 386 to 590degreesC. The characteristic pyrolytic products are cyclohexane homologues. (C) 2002 Wiley Periodicals, Inc. [References: 6]
机译:采用高分辨率热解气相色谱-质谱(HRPyGC-MS)和傅立叶变换红外光谱(FTIR)研究了通过两种不同方法制备的氯化天然橡胶(CNR)的结构。结果表明,由“胶乳”和“溶液”工艺制备的CNR的精细结构不同,而其基本结构相似。来自“胶乳”过程的CNR分子包含一些羧基和羰基。 CNR分子链上的环应为六环。 CNR的最佳热解温度为445摄氏度,可用范围为386至590摄氏度。典型的热解产物是环己烷同系物。 (C)2002 Wiley Periodicals,Inc. [参考:6]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号