Semiflexible random thermotropic copolymers from 8-(3-hydroxy phenyl) octanoic acid and 3-chloro-4-hydroxy benzoic acid/3,5-dibromo-4-hydroxy benzoic acid

机译:8-(3-羟基苯基)辛酸和3-氯-4-羟基苯甲酸/ 3,5-二溴-4-羟基苯甲酸的半柔性无规热致共聚物

获取原文
获取原文并翻译 | 示例
           

摘要

Two series of semiflexible random thermotropic copolymers containing 8-(3-hydroxy phenyl) octanoic acid (HPOA) with either 3-chloro-4-hydroxy benzoic acid or 3,5-dibromo-4-hydroxy benzoic acid were prepared by melt polycondensation techniques. The copolyesters were characterized with Fourier transform infrared spectroscopy, dilute solution viscometry, hot-stage polarized light microscopy, differential scanning calorimetry, thermogravimetric analysis, and wide-angle X-ray diffraction. Studies revealed that the amount of HPOA as a disruptor incorporated into the backbone of substituted 4-hydroxy benzoic acids had a detrimental effect on the liquid-crystalline behavior. Mesophase-transition temperatures were observed between 210 and 250 degrees C, and the optical textures were of typical nematic phases. The degree of crystallinity decreased with an increase in the HPOA content. The thermal stability of the copolymers was in the range of 310-370 degrees C. (C) 2007 Wiley Periodicals, Inc.
机译:通过熔融缩聚技术制备了包含8-(3-羟基苯基)辛酸(HPOA)与3-氯-4-羟基苯甲酸或3,5-二溴-4-羟基苯甲酸的两系列半柔性无规热致共聚物。 。通过傅里叶变换红外光谱,稀溶液粘度测定,热阶段偏振光显微镜,差示扫描量热法,热重分析和广角X射线衍射对共聚酯进行表征。研究表明,掺入取代的4-羟基苯甲酸主链中的作为破坏剂的HPOA的含量对液晶行为有不利影响。在210至250摄氏度之间观察到中间相转变温度,并且光学织构具有典型的向列相。结晶度随着HPOA含量的增加而降低。共聚物的热稳定性在310-370摄氏度的范围内。(C)2007 Wiley Periodicals,Inc.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号