Molybdenum disilicide powders were prepared by heating a mixture of Mo and Si powders with Na metal. The single phases of β-MoSi_2 and α-MoSi_2 powders were obtained at 873 K and 1073K, respectively. The preparation temperature of the single phase á-MoSi_2 powder was 500 K lower than that of the conventional solid state reaction method using Mo and Si powders. The grain size of both MoSi_2 powders was less than 2 ìm, and their shape was angular and irregular.
机译:通过加热钼和硅粉末与金属钠的混合物来制备二硅化钼粉末。 β-MoSi_2和α-MoSi_2粉末的单相分别在873 K和1073K处获得。单相á-MoSi_2粉末的制备温度比使用Mo和Si粉末的常规固态反应方法的制备温度低500K。两种MoSi_2粉末的晶粒尺寸均小于2μm,且形状呈棱角形和不规则形。