首页> 外文期刊>Journal of Applied Polymer Science >Facile preparation and characterization of soluble aramid
【24h】

Facile preparation and characterization of soluble aramid

机译:可溶性芳纶的舒适制备及表征

获取原文
获取原文并翻译 | 示例
           

摘要

It remains a problem to prepare cost-effective aramid with good solubility via a simple method since the commercialization of aromatic polyamides such as Kevlar and Nomex by DuPont in 1960s. Herein, we report the facile preparation and properties of an aromatic polyamide copolymerized by 2,6-naphthalene dichloride (26N-COCl), 4,4-oxydianiline, and m-phenylenediamine. The synthetic route is very facile and cost-effective. The modified aramids possess excellent comprehensive properties. The polymers are soluble in some organics. Their thermal stabilities are excellent, with 5% weight loss temperatures (T-d,T-5%'s) in air higher than 460 degrees C and glass transition temperatures (T-g's) higher than 280 degrees C. These polymers are easily processed into films, fibers, and tubes. The products exhibit high strength. For example, the films have excellent mechanical strength, with a tensile strength up to 139 MPa, a tensile modulus up to 3.45 GPa, and an elongation of 11%. The films are also transparent and fluorescent. The overall properties are better than those of the commercial Nomex. The facilely prepared aramids with good solubility are very promising for commercial use. (c) 2018 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2018, 135, 46341.
机译:在20世纪60年代,通过简单的方法制备具有良好溶解性的成本效率的芳族溶解性,仍然存在良好的溶解性。在此,我们报告了通过2,6-萘二氯化物(26N-COCl),4,4- oxydianiline和M-苯二胺共聚的芳族聚酰胺的容易制剂和性质。合成路线非常适合且成本效益。改良的芳族芳纶具有出色的综合性质。聚合物可溶于一些有机物。它们的热稳定性优异,在高于460℃和高于280℃的玻璃化转变温度(T-G)高于460℃的空气中具有5%的重量损失温度(Td,T-5%)。这些聚合物易于加工薄膜,纤维和管。产品表现出高强度。例如,薄膜具有优异的机械强度,抗拉强度高达139MPa,拉伸模量高达3.45GPa,伸长率为11%。薄膜也是透明和荧光的。整体属性优于商业Nomex。有用的制备的芳族聚酰胺具有良好的溶解度非常有前途的商业用途。 (c)2018 Wiley期刊,Inc.J.Phill。聚合物。 SCI。 2018,135,46341。

著录项

  • 来源
    《Journal of Applied Polymer Science》 |2018年第24期|共10页
  • 作者单位

    Peking Univ Ctr Soft Matter Sci &

    Engn Coll Chem &

    Mol Engn Minist Educ Beijing Natl Lab Mol Sci Key Lab Polymer Chem &

    P Beijing 100871 Peoples R China;

    Chinese Acad Sci Beijing Natl Lab Mol Sci Inst Chem Lab Polymer Phys &

    Chem Beijing 100871 Peoples R China;

    Peking Univ Ctr Soft Matter Sci &

    Engn Coll Chem &

    Mol Engn Minist Educ Beijing Natl Lab Mol Sci Key Lab Polymer Chem &

    P Beijing 100871 Peoples R China;

    Peking Univ Ctr Soft Matter Sci &

    Engn Coll Chem &

    Mol Engn Minist Educ Beijing Natl Lab Mol Sci Key Lab Polymer Chem &

    P Beijing 100871 Peoples R China;

    Chinese Acad Sci Beijing Natl Lab Mol Sci Inst Chem Lab Polymer Phys &

    Chem Beijing 100871 Peoples R China;

    Chinese Acad Sci Beijing Natl Lab Mol Sci Inst Chem Lab Polymer Phys &

    Chem Beijing 100871 Peoples R China;

    Chinese Acad Sci Beijing Natl Lab Mol Sci Inst Chem Lab Polymer Phys &

    Chem Beijing 100871 Peoples R China;

    Chinese Acad Sci Beijing Natl Lab Mol Sci Inst Chem Lab Polymer Phys &

    Chem Beijing 100871 Peoples R China;

    Peking Univ Ctr Soft Matter Sci &

    Engn Coll Chem &

    Mol Engn Minist Educ Beijing Natl Lab Mol Sci Key Lab Polymer Chem &

    P Beijing 100871 Peoples R China;

    Peking Univ Ctr Soft Matter Sci &

    Engn Coll Chem &

    Mol Engn Minist Educ Beijing Natl Lab Mol Sci Key Lab Polymer Chem &

    P Beijing 100871 Peoples R China;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类 高分子化合物工业(高聚物工业);
  • 关键词

    functionalization of polymers; polyamides; structure-property relationships;