The microhardness on the (010) and (001) planes in K2Co(SO4)(2) center dot 6H(2)O crystal has been measured by the Vickers indentation method. Its values are, respectively, 11500 and 1300 MPa. No microhardness anisotropy of the first kind is revealed on either plane. The fracture geometry under indentation by a spherical indenter and Vickers and Knoop indenters is studied. The crystal has lower brittleness than the isomorphic Cs2Ni(SO4)(2) center dot 6H(2)O crystal.
机译:已经通过维氏压痕法测量了K2Co(SO4)(2)中心点6H(2)O晶体在(010)和(001)面上的显微硬度。其值分别为11500和1300MPa。在任何一个平面上都没有揭示出第一类的显微硬度各向异性。研究了球形压头,维氏和努氏压头在压痕下的断裂几何形状。该晶体的脆性低于同构Cs2Ni(SO4)(2)中心点6H(2)O晶体。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号