Corrosion inhibition properties of two imidazolium ionic liquids with hydrophilic tetrafluoroborate and hydrophobic hexafluorophosphate anions in acid medium

机译:酸性介质中含有亲水四氟硼酸盐和疏水性六氟磷酸根阴离子的腐蚀抑制性能

获取原文
获取原文并翻译 | 示例
           

摘要

The ionic liquids, 1-viny1-3-aminopropylimidazolium hexafluorophosphate ([VAIM][PF6]) and 1-vinyl-3-aminopropylimidazolium tetrafluoroborate ([VAIM][BF4]) acted as the corrosion inhibitors. Weight loss measurements showed the corrosion inhibition efficiencies of [VAIM][PF6] and [VAIM][BF4] were 90.53% and 54.01% at 45 degrees C, respectively. The ILs were mix-type inhibitors. Raising the temperature can have a decreased inhibition efficiency of [VAIM][BF4], while [VAIM][PF6] presented an opposite trend. In addition, [VAIM][PF6] obeyed Langmuir monolayer adsorption isotherm, while [VAIM][BF4] obeyed El-Awady kinetic-thermodynamic adsorption for blocking active sites. Moreover, Molecular Dynamic Simulations showed that [VAIM][PF6] owned a higher adsorption energy, which may be responsible for the more adsorption groups of [VAIM][PF6]. (C) 2017 The Korean Society of Industrial and Engineering Chemistry. Published by Elsevier B.V. All rights reserved.
机译:离子液体,1- viny1-3-氨基丙基咪唑鎓六氟磷酸盐([vaim] [PF6])和1-乙烯基-3-氨基丙基咪唑鎓四氟硼酸盐([vaim] [bf4]用作腐蚀抑制剂。 重量损失测量显示[Vaim] [PF6]和[Vaim] [BF4]的腐蚀抑制效率分别分别为45℃的90.53%和54.01%。 ILS是混合型抑制剂。 提高温度可以降低[vaim] [bf4]的抑制效率,而[vaim] [pf6]呈现相反的趋势。 此外,[vaim] [pf6]服从朗米尔单层吸附等温线,而[vaim] [bf4]遵守El-awady动力学热动力吸附,用于阻断活性位点。 此外,分子动态模拟表明,[Vaim] [PF6]拥有较高的吸附能量,这可能负责[Vaim] [PF6]的吸附组。 (c)2017年韩国工程和工程化学学会。 elsevier b.v出版。保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号