Grain Boundary Wetting by a Second Solid Phase in Ti-Fe Alloys

机译:在Ti-Fe合金中第二固相润湿晶粒边界

获取原文
获取原文并翻译 | 示例
           

摘要

The microstructure of Ti-Fe polycrystals has been studied between 595 and 815?°C in the concentration interval between 1 and 9?wt.% Fe. In these conditions, two phases, namely hexagonal α(Ti, Fe) and cubic β(Ti, Fe), are in equilibrium. The α(Ti, Fe) phase forms either continuous or discontinuous layers in the β(Ti, Fe)/β(Ti, Fe) grain boundaries (GBs). Continuous layers correspond to the complete wetting of β(Ti, Fe)/β(Ti, Fe) GBs by a second solid phase α(Ti, Fe). Discontinuous layers correspond to the incomplete (or partial) GB wetting by a second solid phase. The temperature dependences of the portion of completely wetted GBs as well as that of the thickness of continuous GB layer of α(Ti, Fe) phase have been measured. Both values monotonously increase with increasing temperature.
机译:在浓度间隔为1和9的浓度间隔之间研究了Ti-Fe多晶体的微观结构。%Fe。 在这些条件下,两相,即六方α(Ti,Fe)和立方β(Ti,Fe)处于平衡。 α(Ti,Fe)相形成β(Ti,Fe)/β(Ti,Fe)晶界(GBS)中的连续或不连续的层。 连续层对应于第二固相α(Ti,Fe)的β(Ti,Fe)/β(Ti,Fe)Gbs的完全润湿。 不连续的层对应于第二固相润湿的不完全(或部分)GB。 已经测量了完全湿润的GBS部分的温度依赖性以及α(Ti,Fe)相的连续GB层的厚度。 两个值随着温度的增加而单调增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号