A direct method to calculate the tempering response of a tool steel (H13) that exhibits secondary hardening is presented. Based on the traditional method of presenting tempering response in terms of isothermal tempering, we show that the tempering response for a steel undergoing a non-isothermal tempering schedule can be predicted. Experiments comprised (1) isothermal tempering, (2) non-isothermal tempering pertaining to a relatively slow heating to process-temperature and (3) fast-heating cycles that are relevant to tempering by induction heating. After establishing the tempering response of the steel under simple isothermal conditions, the tempering response can be applied to non-isothermal tempering by using a numerical method to calculate the tempering parameter. Calculated results are verified by the experiments.
机译:提出了一种直接方法,用于计算表现出次要硬化的工具钢(H13)的回火响应。 基于在等温回火方面呈现回火响应的传统方法,我们表明,可以预测钢的钢的回火响应。 实验组成(1)等温回火,(2)与相对缓慢的加热有关的非等温回火,以通过感应加热与回火相关的加工温度和(3)快速加热循环。 在简单的等温条件下建立钢的回火响应之后,通过使用数值方法计算回火参数,可以将回火响应施加到非等温的回火。 计算结果通过实验验证。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号