A series of orthophosphate solid solutions with a general formula of Sr8Mg1-mZnmY(PO4)(7): Eu2+ (0 <= m <= 1) were synthesized by the combustion-assisted synthesis technique. The XRD patterns confirm the formation of a solid solution of Sr8Mg1-mZnmY(PO4)(7) and lattice parameters of the solid solutions are linearly dependent on m. The excitation spectra of these phosphors show broad band excitation and absorption in the 250-470 nm near ultraviolet (UV) region, which is ascribed to the 4f(7)-4f(6)5d(1) transitions of Eu2+. With an increase in m, the emission color shifts from yellow to green under near-UV excitation, which is rationalized in terms of two competing factors of the crystal filed strength and bond covalence. All the results indicate that the solid solution Sr8Mg1-mZnmY(PO4)(7): Eu2+ can be a good candidate of phosphor applicable to near-UV LEDs for solid-state lighting.
机译:通过燃烧辅助合成技术合成了一系列通式为Sr8Mg1-mZnmY(PO4)(7):Eu2 +(0 <= m <= 1)的正磷酸盐固溶体。 X射线衍射图谱证实了Sr8Mg1-mZnmY(PO4)(7)固溶体的形成,且固溶体的晶格参数与m线性相关。这些荧光粉的激发光谱在250-470 nm附近的紫外(UV)区域显示宽带激发和吸收,这归因于Eu2 +的4f(7)-4f(6)5d(1)跃迁。随着m的增加,在近紫外线激发下,发射颜色从黄色变为绿色,这是根据晶体场强度和键合价的两个竞争因素合理化的。所有结果表明,固溶体Sr8Mg1-mZnmY(PO4)(7):Eu2 +可能是适用于固态照明的近紫外LED的良好荧光粉候选者。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号