To provide a recycled asphalt mixture manufacturing method and recycled asphalt mixture capable of exhibiting further excellent durability.SOLUTION: A recycled asphalt mixture manufacturing method includes the steps of: adding a regeneration additive and/or a workability improving agent to an asphalt recycled aggregate a by an injector at normal temperature or by heating; and curing the asphalt recycled aggregate a for 3 days or more. Thereby, the regeneration additive and/or the workability improving agent penetrate(s) deeply into the old asphalt and improve(s) the properties of the asphalt recycled aggregate a. The cured asphalt recycled aggregate a is dried by heating. Then, the asphalt recycled aggregate a is charged into a mixer 5 together with a novel coarse aggregate b, a fine aggregate d, a filler such as stone powder, and a novel asphalt c, and mixed, whereby a recycled asphalt mixture A can be manufactured.SELECTED DRAWING: Figure 1
机译:为了提供一种再生沥青混合料的制造方法和能够表现出进一步优异耐久性的再生沥青混合料。常温或加热下的注射器;然后将沥青再生骨料固化3天或更长时间。从而,再生添加剂和/或可加工性改进剂深深地渗透到旧沥青中,并改善了沥青再生集料a的性能。固化的沥青回收的骨料a通过加热干燥。然后,将沥青再生集料a与新型粗集料b,细集料d,填料如石粉和新型沥青c一起加入混合机5中,并进行混合,从而可以将再生沥青混合物A制成选定的图纸:图1

著录项

  • 公开/公告号JP2020037798A

    专利类型

  • 公开/公告日2020-03-12

    原文格式PDF

  • 申请/专利权人 NIPPO CORP;

    申请/专利号JP20180164924

  • 申请日2018-09-03

  • 分类号E01C19/10;

  • 国家 JP

  • 入库时间 2022-08-21 11:37:41

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号