首页> 外国专利> Method of evaluating battery characteristics using non-aqueous electrolyte coin type battery and method of evaluating battery characteristics of positive electrode active material for non-aqueous electrolyte secondary battery

Method of evaluating battery characteristics using non-aqueous electrolyte coin type battery and method of evaluating battery characteristics of positive electrode active material for non-aqueous electrolyte secondary battery

机译:使用非水电解质硬币型电池的电池特性的评价方法以及非水电解质二次电池用正极活性物质的电池特性的评价方法

摘要

PROBLEM TO BE SOLVED: To provide a characteristic evaluation method of a positive electrode active material for a nonaqueous electrolytic secondary battery, in which an evaluation condition can be controlled, and the AC impedance measurement and initial charge/discharge capacity measurement can be concurrently evaluated with stability and good accuracy.SOLUTION: A battery characteristic evaluation method by using a nonaqueous electrolyte coin-type battery with an electrode part having a positive and negative electrode films facing each other through a separator, provided that the positive electrode film includes a positive electrode active material consisting of a Li-Ni composite oxide having a high Ni content and expressed by the general formula, LiNiCoMOcomprises steps of: preparing the nonaqueous electrolyte coin-type battery; performing a constant-current charge/discharge cycle including a constant-current charge, a suspension and then a constant-current discharge to measure an initial charge/discharge capacity after stationarily leaving the battery; and then, going through a suspension time and charging the battery with a constant current and a constant voltage to perform a resistance measurement by an AC impedance method within one hour after the end of the constant-current, constant-voltage charging.SELECTED DRAWING: None
机译:解决的问题:提供一种非水电解质二次电池用正极活性物质的特性评价方法,其中,可以控制评价条件,并且可以同时评价交流阻抗测定和初期充放电容量测定。解决方案:使用非水电解质硬币型电池的电池特性评估方法,该非水电解质硬币型电池的电极部分具有通过隔离膜彼此面对的正极膜和负极膜,但前提是正极膜必须包含正极活性物质LiNiCoMO由具有高Ni含量并由通式表示的Li-Ni复合氧化物组成的材料包括以下步骤:制备非水电解质硬币型电池;进行包括恒流充电,悬浮,然后恒流放电的恒流充电/放电循环,以静态测量离开电池后的初始充电/放电容量;然后,经过一段暂停时间,并在恒流恒压充电结束后一小时内,以恒定电流和恒压对电池充电,以通过AC阻抗法进行电阻测量。没有

著录项

  • 公开/公告号JP6541035B2

    专利类型

  • 公开/公告日2019-07-10

    原文格式PDF

  • 申请/专利权人 住友金属鉱山株式会社;

    申请/专利号JP20150254956

  • 发明设计人 尾崎 光;

    申请日2015-12-25

  • 分类号H01M10/0585;H01M4/525;H01M4/505;H01M10/052;G01R31/378;G01R31/387;G01R31/389;

  • 国家 JP

  • 入库时间 2022-08-21 12:19:28