Provided is a process for producing calcium carbide granules which, when used for dry-process acetylene generation, neither enhance side reactions such as acetylene polymerization, nor adversely affect the yield, nor enhance the risk to safety due to an increase in reaction temperature. The process is for producing calcium carbide granules in which the content of granules having a diameter of 4 mm or larger is 5 wt.% or less and the content of granules having a diameter of 0.15 mm or smaller is 20 wt.% or less, the process comprising the step (A) of crushing calcium carbide with a crusher, the step (B) of putting the calcium carbide which has been crushed with the crusher through a screen having an opening size of 4 mm, and the step (C) of introducing the calcium carbide remaining on the screen into the crusher again. The steps (A) to (C) are conducted in an inert gas atmosphere. The size of crushed granules to be obtained by the crusher is controlled so that the amount of the calcium carbide introduced into the crusher in the step (A), a, and the amount of the calcium carbide passing through the screen in the step (B), b, satisfy 1‰¤(a-b)/b‰¤2.5.
机译:提供了一种生产电石颗粒的方法,当该电石颗粒用于干法乙炔生产时,既不会增强副反应,例如乙炔聚合,也不会不利地影响产率,也不会由于反应温度的升高而增加安全风险。该方法用于制备电石颗粒,其中直径为4mm或更大的颗粒的含量为5wt。%或更少,直径为0.15mm或更小的颗粒的含量为20wt。%或更少,该方法包括以下步骤:通过破碎机破碎电石的步骤(A),将通过破碎机破碎的电石通过开口尺寸为4mm的筛子的步骤(B)和步骤(C)将残留在筛网上的电石再次引入破碎机的方法。步骤(A)至(C)在惰性气体气氛中进行。控制通过破碎机获得的破碎颗粒的尺寸,以使得在步骤(A)中引入到破碎机中的电石的量a和在步骤(B)中通过筛网的电石的量。 ),b,满足1‰¤(ab)/b‰¤2.5。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号