摘要

In dry acetylene generator, or to increase the byproduct reaction of acetylene polymerization such, without adversely affecting the yield and also not to invite Zocho risks for security due to the reaction temperature increases, the calcium carbide particle production method I provide. Calcium carbide method of greater than or equal to the particle diameter 4mm or less 5wt% and the particle size of 0.15mm or less to produce a 20wt% or less of calcium carbide grains, and a step A of pulverizing the calcium carbide in the crusher, it is pulverized by a pulverizer The comprises a step B of MeHiraki is applied to 4mm sieve, and a step C of introducing the remaining calcium carbide on the sieve again to the mill. Said step A~C is carried out in an inert gas atmosphere. The calcium carbide amount a to be introduced to the grinding machine in the step A, the calcium carbide content b having passed through the sieve in the step B is such that (a-b) /b=1~2.5, the grinding It wants to control the grinding particle size by machine.
机译:在干乙炔发生器中,或者为了增加乙炔聚合的副产物反应,而不会不利地影响产率并且也不会由于反应温度的升高而引起Zocho的安全性风险,我提供了一种电石颗粒生产方法I。粒径大于等于4mm或小于5wt%且粒径小于或等于0.15mm的碳化钙法以产生小于等于20wt%的碳化钙晶粒,以及在破碎机中将碳化钙粉碎的步骤A包括将MeHiraki的步骤B施加到4mm筛上,以及将筛上剩余的碳化钙再次引入到研磨机中的步骤C。所述步骤A〜C在惰性气体气氛中进行。要在步骤A中引入到研磨机中的电石量a,在步骤B中通过筛子的电石含量b为(ab)/b=1~2.5,则要进行研磨机器的研磨粒度。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号