PROBLEM TO BE SOLVED: To provide a blast furnace slow cooling slag roadbed material capable of inhibiting generation of expansive sulfate hydrate without modifying blast furnace slow cooling slag using large-scale facilities for desulfurization, controlled cooling from high temperature, and the like, without adding expensive reagents, and without impairing strength, and to provide a method for manufacturing a blast furnace slow cooling slag roadbed material and a method for constructing a blast furnace slow cooling slag roadbed material.;SOLUTION: In a blast furnace slow cooling slag roadbed material according to the present invention, one or two or more additive materials containing at least one of water-soluble silica, water-soluble iron and a water-soluble magnesium are mixed into blast furnace slow cooling slag.;SELECTED DRAWING: None;COPYRIGHT: (C)2016,JPO&INPIT
机译:解决的问题:使用大型脱硫设备,可控的高温冷却等,不添加而提供一种高炉缓冷渣路基材料,其能够抑制膨胀硫酸盐水合物的产生而无需改变高炉缓冷渣。昂贵的试剂,且不会损害强度,并提供一种高炉缓冷渣路基材料的制造方法和一种高炉缓冷渣路基材料的制造方法。在本发明中,将含有水溶性二氧化硅,水溶性铁和水溶性镁中的至少一种的一种或两种以上的添加剂材料混入高炉缓冷渣中。 C)2016,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号