MANUFACTURING METHOD OF ECHO MORTAR/CONCRETE IN LOESS GARDEN AND A MANUFACTURING METHOD OF NON-SINTERED BLOCK/PLATE STONE BY USING THE SAME CAPABLE OF REINFORCING COMPRESSIVE STRENGTH AND BOND STRENGTH OF LOESS MATERIALS

机译:黄土花园回声砂浆/混凝土的制造方法与无粘结砌块板的制造方法-兼论黄土材料的抗压强度和粘结强度。

摘要

PURPOSE: A manufacturing method of echo mortar/concrete in loess garden and a manufacturing method of non-sintered block/plate stone by using the same are provided to prevent generation of harmful material from construction materials and sick house syndromes.;CONSTITUTION: A manufacturing method of non-sintered block/plate stone comprises the following steps: mixing environmentally-friendly loess material, environmentally-friendly remitar, and environmentally-friendly concrete with water; installing the mixture; and non-sintering thereof in order to manufacture the block/plate stone. The environmentally-friendly loess material comprises 7.5±2.5 wt% of natural glue, 25±5 wt% of natural gypsum, and 67.5±7.5 25±5 wt% of loess powder. The environmentally-friendly remitar comprises 36.5±3.5 wt% of the environmentally-friendly loess material and 63.5±3.5 wt% of sand. A manufacturing method of the environmentally-friendly mortar comprises the following step: mixing the environmentally-friendly remitar with water.;COPYRIGHT KIPO 2013;[Reference numerals] (1) Environmentally-friendly glue; (2) Natural environmentally-friendly loess cement(cement substitute); (3) Environmentally-friendly remitar; (4) Environmentally-friendly mortar; (5) Environmentally-friendly cone; (6) Environmentally-friendly block; (7) Environmentally-frienly flagstone(aggregate is not included); (AA) Sign marking; (BB) Environmentally-friendly glue; (CC) Gypsum; (DD) Gravel; (EE) Loess; (FF) Sand; (GG) Water
机译:目的:提供一种在黄土花园中回声砂浆/混凝土的制造方法以及一种使用非回火砂浆/混凝土的制造方法,以防止建筑材料和病房综合症产生有害物质。非烧结块/板石的方法包括以下步骤:将环保的黄土材料,环保的胶浆和环保的混凝土与水混合;安装混合物;并对其进行非烧结以制造块/板石。环保型黄土材料包括7.5%至2.5 wt%的天然胶,25%至5 wt%的天然石膏和67.5%7.5 25至5 wt%的黄土粉。环保型胶合料占环保型黄土材料的36.5%〜3.5 wt%和砂土的63.5%〜3.5 wt%。环保砂浆的制造方法包括以下步骤:将环保涂料与水混合。; COPYRIGHT KIPO 2013; [参考数字](1)环保胶; (2)天然环保黄土水泥(水泥替代品); (3)环保汇款机; (4)环保砂浆; (5)环保锥; (六)环保街区; (七)环保石板(不含骨料); (AA)标志标记; (BB)环保胶; (CC)石膏; (DD)碎石; (EE)黄土; (FF)沙; (GG)水

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号