首页> 外国专利> Low temperature co-fired ceramic material, low temperature co-fired ceramic body, and multilayer ceramic substrate

Low temperature co-fired ceramic material, low temperature co-fired ceramic body, and multilayer ceramic substrate

机译:低温共烧陶瓷材料,低温共烧陶瓷体和多层陶瓷基板

摘要

A low temperature co-fired ceramic material includes a SiO2—BaO—Al2O3-based primary component, and, as secondary components, 0.044 to 0.077 parts by weight of iron in terms of Fe2O3 and 0.30 to 0.55 parts by weight of zirconium in terms of ZrO2 relative to 100 parts by weight of the SiO2—BaO—Al2O3-based primary component. The SiO2—BaO—Al2O3-based primary component preferably includes 47% to 60% by weight of SiO2, 20% to 42% by weight of BaO, and 5% to 30% by weight of Al2O3.
机译:一种低温共烧陶瓷材料,包括基于SiO 2 -BaO-Al 2 O 3 的主要成分,并作为辅助成分,以Fe 2 O 3 计为0.044至0.077重量份的铁,以ZrO 2 相对于基于SiO 2 -BaO-Al 2 O 3 的主要成分100重量份。基于SiO 2 -BaO-Al 2 O 3 的主要组分优选包含按重量计47%至60%的SiO 2 ,按重量计20%至42%的BaO和按重量计5%至30%的Al 2 O 3

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号