There is provided a soil hardening method, a soil solidification method and a soft ground solidification method for replacing road pavement aggregates using the same.;This soil hardening agent is in weight percent, calcium chloride: 11-18%, lignin sulfonate: 15-25%, tripolylate: 13-20%, ferrous lactate: 7-18%, stearic acid salt: 5-11%, Soil hydroxide: 12 to 20%, magnesium chloride: 15 to 25%, calcium oxide: 8 to 12% of the raw material for the soil hardening agent is mixed 3 to 15 parts by weight with respect to 100 parts by weight of cement.;According to the present invention, it is possible to provide an environmentally friendly soil hardener that can replace the aggregate in the lower road pavement with soil. In addition, the solidification method of the present invention can provide a secure ground that is capable of rapid solidification treatment, has excellent uniaxial compressive strength, and does not settle, and this solidification method can be applied to soft ground and the like.;Soil hardening, road paving, solidification, soft ground, uniaxial compressive strength, ferrous lactic acid
机译:提供了一种土壤硬化方法,一种土壤固化方法以及一种使用该方法来代替道路路面集料的软土地基固化方法。该土壤硬化剂的重量百分比为:氯化钙:11-18%;木质素磺酸盐:15- 25%,三聚酸酯:13-20%,乳酸亚铁:7-18%,硬脂酸盐:5-11%,土壤氢氧化物:12至20%,氯化镁:15至25%,氧化钙:8至12%相对于100重量份的水泥,将3重量份的土壤硬化剂的原料混合3至15重量份。根据本发明,可以提供一种环境友好的土壤硬化剂,其可以代替骨料中的骨料。较低的路面铺有土壤。另外,本发明的固化方法可以提供能够快速固化处理,具有优异的单轴抗压强度并且不沉降的牢固的地面,并且该固化方法可以应用于软地面等。硬化,铺路,固化,软土地基,单轴抗压强度,乳酸亚铁

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号