Piezoelectric properties with a composition of 0.05 Pb (Mn 1/3 Sb 2/3 ) O 3 -0.95Pb (Zr, Ti) O 3 -x (mol%) ZnO-1 (wt%) PbO (0≤x≤5) This excellent PMS-PZT ceramic is provided. The manufacturing method consists of the following steps. 0.05 Pb (Mn 1/3 Sb 2/3 ) O 3 -0.95Pb (Zr, Ti) O 3 -x (mol%) ZnO-1 (wt%) PbO (0≤x≤5) Preparing raw powders of ZrO 2 , TiO 2 , MnO 2 , Sb 2 O 3 and ZnO; Forming a dry powder from the raw powder; Classifying the dry powder and then calcining; Supplying an additive and a binder to the calcined powder and then drying it; Pressure molding the dried powder to form a molded body; And sintering the molded body in an atmosphere of the same composition.;PMS-PZT, Piezoelectric Ceramic
机译:组成为0.05 Pb(Mn 1/3 Sb 2/3 )O 3 -0.95Pb(Zr,Ti)O的压电性能 3 -x(mol%)ZnO-1(wt%)PbO(0≤x≤5)提供了这种出色的PMS-PZT陶瓷。该制造方法包括以下步骤。 0.05 Pb(Mn 1/3 Sb 2/3 )O 3 -0.95Pb(Zr,Ti)O 3 -x(mol%)ZnO-1(wt%)PbO(0≤x≤5)制备ZrO 2 ,TiO 2 ,MnO 2 ,Sb 2 O 3 和ZnO;从原料粉末中形成干燥粉末;分类干粉,然后煅烧;向煅烧的粉末中加入添加剂和粘合剂,然后干燥;将干燥的粉末加压成型以形成成型体;并在相同组成的气氛中烧结成型体。; PMS-PZT,压电陶瓷

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号