PROBLEM TO BE SOLVED: To provide a manufacturing method of 2-17 based SmCo permanent magnet powder, 2-17 based SmCo permanent magnet powder obtained by the manufacturing method, and a bonded magnet obtained by using the 2-17 based SmCo permanent magnet powder. ;SOLUTION: The composition of 2-17 based SmCo permanent magnet powder is comprises R of 25.0-26.5% (where R is one kind or combination of at least two kinds of rare earth elements, with Sm at the center), Fe of 17.0-21.0%, Cu of 7.0-8.5%, Zr of 1.8-2.3%, and residual % of Co and inevitable impurities, when they are shown by weight percentage. In a nonoxidative atmosphere, by using permanent magnet alloy ingot manufactured by a strip cast method, solution treatment at 1,100-1,180°C and isothermal aging treatment at 750-900°C are performed. Continuously, slow cooling as far down as a temperature lower than or equal to 500°C, and isothermal aging treatment at 500°C or lower or a multistage aging treatment as far as a temperature lower than or equal to 500°C are performed. After that, rough grinding and fine grinding are performed, and permanent magnet powder is obtained.;COPYRIGHT: (C)2001,JPO
机译:解决的问题:提供一种2-17基SmCo永磁体粉末的制造方法,通过该制造方法获得的2-17基SmCo永磁体粉末和通过使用2-17基SmCo永磁体粉末获得的粘结磁体。 。 ;解决方案:2-17基SmCo永磁粉末的成分包含25.0-26.5%的R(其中R为一种或至少两种稀土元素的组合,Sm为中心),Fe为17.0当以重量百分比表示时,它们为-21.0%,Cu为7.0-8.5%,Zr为1.8-2.3%,以及Co和不可避免的杂质的残留%。在非氧化性气氛中,通过使用通过薄带铸造法制造的永磁合金锭,进行在1100-1180℃的固溶处理和在750-900℃的等温时效处理。连续地,进行直到温度低于或等于500℃的缓慢冷却,以及在500℃或更低的温度下进行等温时效处理,或者进行直到温度低于或等于500℃的多阶段时效处理。之后,进行粗磨和精磨,得到永磁体粉末。;版权所有:(C)2001,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号