Refractory inorganic fiber of al deep 2 o deep 3, cr deep 2 o deep 3, ro deep 2 with at least a microcrystalline phase and a method for their preparation

机译:至少具有微晶相的Al深2 o深3,cr深2 o深3,ro深2的耐火无机纤维及其制备方法

摘要

Refractory fibers having a composition of 10-75% Al2O3, 1-30% Cr2O3 and 10-75% metal (IV) oxide selected from at least one of silica, titania, zirconia, and tin oxide and having at least one microcrystalline phase therein may remain strong, flexible, and continuous at temperatures of 1300 DEG to 1500 DEG C and beyond.
机译:耐火纤维,其成分为10-75%Al2O3、1-30%Cr2O3和10-75%的金属(IV)氧化物,选自二氧化硅,二氧化钛,氧化锆和氧化锡中的至少一种,并且其中至少有一种微晶相在1300℃至1500℃及更高的温度下可以保持坚固,柔韧性和连续性。

著录项

  • 公开/公告号DE2432434B2

    专利类型

  • 公开/公告日1977-07-21

    原文格式PDF

  • 申请/专利权人

    申请/专利号DE19742432434

  • 发明设计人

    申请日1974-07-04

  • 分类号C03C13/00;C04B35/42;

  • 国家 DE

  • 入库时间 2022-08-23 00:07:19

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号