NMR Study of Poly(γ-Glutamic Acid) and Partially Benzylated Poly (γ-Glutamic Acid): Nanoparticles in Solution

机译:聚(γ-谷氨酸)和部分苄基化聚(γ-谷氨酸)的NMR研究:溶液中的纳米粒子

获取原文

摘要

Poly(γ-glutamic acid) (γ-PGA) and its partially benzylami-dated (hydrophobized) derivatives were prepared and studied in solution by means of dynamic light scattering (DLS), ID, 2D and PGSE NMR in order to determine the structure, size and aggregation in solution. By pH potentiometric titrations in aqueous solution the apparent pK ≈ 4 of γ-PGA was determined. The measured diffusion coefficients as a function of pH showed the swelling of γ-PGA by deprotonation of carboxyls. DLS measurements showed a certain degree of aggregation even in dilute solution. The degree of aggregation is increased in the presence H_2PO_4-and HPO_4~(2-) buffer anions. Benzylamidation of 30-50% of caboxylates resulted in folded structure of the BzPGA, probably spherical like nanoparticles, verified by NMR diffusiometry and 2D NOE spectroscopy.
机译:通过动态光散射(DLS),ID,2D和PGSE NMR制备聚(γ-谷氨酸)(γ-PGA)及其部分苄基致氧化(疏水化)衍生物,并在溶液中研究,以确定结构解决方案中的大小和聚合。通过pH水溶液中的pH电位滴定,测定表观pk≈4的γ-pga。测量的扩散系数作为pH的函数,通过羧基的去质子显示γ-PGA的溶胀。即使在稀释溶液中,DLS测量也表现出一定程度的聚集。在存在H_2PO_4和HPO_4〜(2-)缓冲阴离子中,聚集程度增加。苄基酰胺化30-50%的Caboxyly导致BZPGA的折叠结构,可能是球形的纳米颗粒,通过NMR扩散测定法和2D NOE光谱验证。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号