Recovery and Grain Growth in a 2% Si - 0.3% Al - 0.003%C Steel

机译:2%Si-0.3%Al-0.003%C钢中的回收率和晶粒长大

获取原文
获取原文并翻译 | 示例
           

摘要

The scope of our investigation covered the effect of carbon on the processes of recovery and grain growth in cold-rolled non-oriented silicon steel, of laboratory and industrial provenance. Decarburized and non-decarburized cold-rolled electrical steels were annealed in a deoxidized lead bath in the temperature range from 550 to 800°C. The microstructuie was examined and average grain size assessed. The process of recovery was investigated on specimens annealed at lower temperatures by measurement of hardness. Industrially manufactured samples of non-oriented sheet were used for comparison. The sheets of both industrial and laboratory manufacture were decarburized by annealing in wet hydrogen with different dew points at temperatures ranging from 800 to 860°C. The rate of decarburization was controlled by chemical analysis of carbon.
机译:我们的研究范围包括碳对实验室和工业来源的冷轧无取向硅钢的恢复和晶粒长大过程的影响。将脱碳和未脱碳的冷轧电工钢在550至800°C的脱氧铅浴中进行退火。检查了微结构并评估了平均晶粒尺寸。通过在较低温度下退火的样品,通过测量硬度来研究恢复过程。使用工业生产的无取向片样品进行比较。通过在温度范围为800至860°C的不同露点的湿氢气中退火,对工业和实验室制造的板材进行脱碳处理。通过碳的化学分析控制脱碳速率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号