The temperature and magnetic field dependence of the radio-frequency (RF) transverse susceptibility (χ_T) of La_(0.67)Ca _(0.33)MnO_3 crystalline nanowires has been studied using a very sensitive self-resonant tunnel-diode oscillator (TDO) technique. The nanowires were synthesized using porous templates of anodized alumina by chemical solution deposition technique, and the crystalline nature of the nanowires with the average diameter of 70 nm was confirmed by TEM, SAED, and HREM. RF transverse susceptibility experiments reveal the presence of a double-peak structure at T≤245 K (the Curie temperature) but a single peak at T>245 K. This distinguishes the low temperature ferromagnetic state from the high temperature paramagnetic state. The effective magnetic anisotropy field (H_K), which corresponds to the peak location of χ_T, has been found to increase with decrease in temperature from the Curie temperature.
机译:使用非常敏感的自谐振隧道二极管振荡器(TDO)技术研究了La_(0.67)Ca _(0.33)MnO_3晶体纳米线的射频(RF)横向磁化率(χ_T)的温度和磁场依赖性。使用化学溶液沉积技术使用阳极氧化铝的多孔模板合成纳米线,并通过TEM,SAED和HREM证实平均直径为70 nm的纳米线的晶体性质。射频横向磁化率实验表明,在T≤245K(居里温度)存在双峰结构,但在T> 245 K处存在一个峰。这将低温铁磁状态与高温顺磁状态区分开。已经发现,对应于χ_T峰值位置的有效磁各向异性场(H_K)随着温度从居里温度降低而增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号