DNA-wrapped halloysite nanotubes were obtained by a mechanochemical reaction in the solid state. The characterization by scanning electron microscopy showed that the nanotubes were cut into shorter lengths and were completely covered with DNA. This resulted in a high aqueous solubility of the product with stability of the solution for about 6 weeks. The nanotubes were cut to different fractions with lengths of 200-400 nm (30-40%), 400-600 nm (10-20%) and 600-800 nm (5-10%) after ball milling. FTIR spectroscopic analysis shows that the DNA in the product remained intact. This straightforward technique for obtaining water-soluble halloysite nanotubes by a solid-state reaction has great potential for biomedical applications of nanotubes.
机译:通过固态的机械化学反应获得了DNA包裹的埃洛石纳米管。通过扫描电子显微镜的表征表明,纳米管被切成较短的长度并被DNA完全覆盖。这导致产物具有高的水溶性,并且溶液具有约6周的稳定性。球磨后,将纳米管切成不同的部分,长度分别为200-400 nm(30-40%),400-600 nm(10-20%)和600-800 nm(5-10%)。 FTIR光谱分析表明产物中的DNA保持完整。通过固相反应获得水溶性埃洛石纳米管的直接方法对于纳米管的生物医学应用具有巨大的潜力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号