SDA Low cost and Hi-performance Asphalt Binder Composition for Asphalt Pavement Using Residue produced during Solvent De-Asphalting Process And Manufacturing Method thereof

机译:用溶剂脱沥青过程中产生的残留物的sda低成本高性能沥青混合料及其制造方法

摘要

The present invention relates to a low-cost and high-performance asphalt mixed composition for asphalt pavement by mixing an asphalt binder composition made using remnants produced through a SDA process (Solvent De-Asphalting Process / solvent deasphalting process or solvent extraction process) And an asphalt mixed composition made thereby.In the present invention, 2 to 8% by weight of an asphalt binder composition produced using the residue of the SDA process; And 92 to 98% by weight of aggregate. The asphalt binder composition according to the present invention is characterized in that the asphalt binder composition contains 100% by weight of the total weight of the asphalt binder composition , 1.0 to 3.0% by weight of at least one material selected from the group consisting of 90 to 95% by weight of residues of the SDA process, 1 to 7% by weight of modifying additives, 0.1 to 1.0% by weight of bonding adjuvant, SBR and SBS, 0.1 to 1.0% by weight of sulfur, and 0.1 to 0.5% by weight of a vulcanization accelerator.
机译:本发明涉及一种低成本高性能沥青混合料组合物,其通过混合使用通过SDA工艺(溶剂脱沥青工艺/溶剂脱沥青工艺或溶剂提取工艺)生产的残余物制备的沥青粘合剂组合物和在本发明中,使用SDA方法的残余物生产的沥青粘合剂组合物的重量为2-8%。占骨料的92-98%(重量)。根据本发明的沥青粘合剂组合物的特征在于,沥青粘合剂组合物包含占沥青粘合剂组合物总重量的100重量%,1.0至3.0重量%的选自由90组成的组的至少一种材料。 SDA工艺中残留物的重量百分比为95%,改性添加剂的重量百分比为1%至7%,粘结助剂,SBR和SBS的重量百分比为0.1至1.0%,硫的重量百分比为0.1至1.0%,0.1%至0.5%按硫化促进剂的重量计。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号