Blends of natural rubber latex and methyl methacrylate-grafted rubber latex

机译:天然胶乳和甲基丙烯酸甲酯接枝的胶乳的混合物

获取原文
获取原文并翻译 | 示例
           

摘要

By mixing natural rubber latex uniformly with methyl methacrylate-grafted natural rubber latex and then carrying out prevulcanization, we obtained blends with stable viscosities. Under certain blending ratios, the blends maintained good basic properties, and the heat stability time (T,,,) of the blend increased with the increment of percent content of MG49 latex (C). The relationship between T,,, and C was T-HS = 0.36C + 33.0, whereas, the mechanical stability time (T-MS) was slightly decreased, and the relationship between T-MS and C was T-MS = -1.33C + 772.0; The modulus, antiaging properties, and tear strength of the films of the blends increased with the increment of C; the tensile strengths fluctuated on a small scope; the Shore A hardness (H) and breaking set (B,) both increased with the increment or C; their relationships were H = 0.66C + 40.0 and B-S = 0.46C + 8.0, respectively. (C) 2002 Wiley Periodicals, Inc. [References: 5]
机译:通过将天然橡胶胶乳与甲基丙烯酸甲酯接枝的天然橡胶胶乳均匀混合,然后进行预硫化,我们获得了具有稳定粘度的共混物。在一定的混合比下,共混物保持良好的基本性能,并且随着MG49胶乳(C)含量百分比的增加,共混物的热稳定时间(T ,,,)增加。 T,C与C的关系为T-HS = 0.36C + 33.0,而机械稳定时间(T-MS)略有减少,T-MS与C的关系为T-MS = -1.33 C + 772.0;共混物薄膜的模量,抗老化性能和撕裂强度随C的增加而增加;抗张强度在很小的范围内波动;肖氏A硬度(H)和断裂形变(B,)均随C的增加而增加;它们的关系分别为H = 0.66C + 40.0和B-S = 0.46C + 8.0。 (C)2002 Wiley Periodicals,Inc. [参考:5]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号